Moldes para fundición a presión a baja presión (LP
Moldes de fundición por gravedad
Moldes de fundición por contrapresión (CPC)
Molde para la fundición de piezas estructurales
Molde de fundición para cubos de rueda de motocicl
Molde de fundición por presión para el diferencial
Molde para la fundición por gravedad del cubo de r
Baja presión en el cubo de la rueda
Selection of PVD coating for die-casting molds: AlTiN, TiN, DLC, applicable scenarios, lifespan, contraindications
PVD is the core method for improving the anti sticking aluminum and wear resistance of mold cavities, gates, and sliders. Many people blindly choose coatings, which can accelerate failure if the working conditions are not matched.
1、 TiN (titanium nitride, golden color)
Basic model, moderate hardness, high temperature resistance of about 450 ℃; Suitable for low temperature and wear based working conditions; Die casting high-temperature cavities are prone to softening, and die casting rarely uses main coatings, but is mostly used for ejector pins and guide sleeves.
2、 AlTiN (aluminum titanium nitride, black purple/gray black, preferred for die casting)
High temperature resistance of 800-900 ℃, generating aluminum oxide isolation film at high temperatures, resistant to aluminum adhesion and thermal fatigue; Suitable for A356, ADC12 cavities, sprues, slider sealing surfaces, and mainstream wheel hub molds.
3、 DLC (Diamond like Coating)
Extremely low friction coefficient, strong anti sticking effect; Shortcoming: Poor heat resistance, coating decomposition exceeding 300 ℃; Can only be used in low-temperature areas: ejector pins, inserts, * * strictly prohibited for high-temperature sprues, cavity working surfaces * *.
4、 Pre conditions for coating
Mirror polishing is required before coating; Cracks, erosion, and pitting need to be repaired first; The coating thickness is only 2-5 μ m and cannot be used to repair dimensions; Coatings cannot replace the heat treatment of the substrate steel.
5、 Coating Failure Modes
Coating peeling and flaking: poor polishing of the substrate, white layer, and inadequate cleaning; Coating wear: Strong flushing of gates by aluminum liquid; High temperature oxidation: Choosing the wrong coating's upper limit for temperature resistance.
6、 Key points of foreign trade quotation
AlTiN is a standard option for die-casting; DLC separately indicates the applicable location; Clearly define the coating quality assurance mold number, distinguish the different lifetimes of the mold cavity, sprue, and ejector pin. Google's "PVD coating AlTiN TiN DLC for die casting mold" is aimed at mold engineers.
FAQ
Does having an AlTiN coating prevent aluminum from sticking?
Significantly reduced, but uncontrolled mold temperature and low iron content in the aluminum liquid will still stick to the aluminum.
Can the coating be directly recoated after wear and tear?
First, polish and remove the old coating, otherwise poor adhesion may cause peeling.
Can AlTiN be used on A356 wheels?
It is the most commonly used coating for A356 wheel hub molds.
Why can't DLC be placed in the sprue?
The gate temperature far exceeds 300 ℃, and DLC directly decomposes and fails.
Can it still be polished after coating?
Light throwing is fine, throwing off the coating will result in loss of protection.
Can different coatings be applied to different positions of the same mold?
Sure, gate cavity AlTiN, ejector pin DLC.
Will the coating affect the surface roughness of the casting?
The qualified coating is extremely thin and basically inherits the polished Ra.
Why do low-priced molds omit coatings?
Save costs, reduce the lifespan of the mold by half, and increase the risk of aluminum adhesion and strain.
MOLDES DE FUNDICIÓN A BAJA PRESIÓN (LPDC)
MOLDES DE FUNDICIÓN POR GRAVEDAD
MOLDES DE FUNDICIÓN POR CONTRAPRESIÓN (CPC)
MOLDES DE FUNDICIÓN DE PIEZAS ESTRUCTURALES
MOLDE DE FUNDICIÓN PARA CUBOS DE RUEDA DE MOTOCICLETA
MOLDE DE FUNDICIÓN POR PRESIÓN DIFERENCIAL PARA CUBOS DE RUEDA
MOLDE DE FUNDICIÓN POR GRAVEDAD PARA CUBOS DE RUEDA
MOLDE DE FUNDICIÓN A BAJA PRESIÓN PARA CUBOS DE RUEDA
MOLDES PARA LLANTAS DE AUTOMÓVIL
PIEZAS ESTRUCTURALES PARA AUTOMÓVILES
OTROS COMPONENTES DE FUNDICIÓN DE ALUMINIO
NOTICIAS DE LA EMPRESA
NOTICIAS DEL SECTOR
BLOG TÉCNICO
PREGUNTAS FRECUENTES PERFIL DE LA EMPRESA
ESTRUCTURA ORGANIZATIVA
HISTORIA DE LA EMPRESA
PROPIEDAD INTELECTUAL
ESPÍRITU DE EQUIPO SOCIOS
Copyright © Zhejiang Xinfeng Machinery Co., Ltd. Todos los derechos reservados.